I am working on a paintball marker and very new to hydro dip. I've been using a test part but having difficulty getting the final result to work. My assumption is that my prep work isn't correct. I'm hoping someone on the forums here can give me an idea on the prep work. I have not been using primer paint just base coat. My process is as follows:

Clean Part Soap & Water
Sand Part 400 Grit
Clean Part Again Soap & Water
Spray Base Coat On 5-10 minute wait
Spray Second Coat On 30 minute wait
Prep Water
Lay Print Down
Spray Activator
Dip